Grade |
2.4952 |
Nimonic 80A |
|
C |
0.04~0.10 |
≤0.10 |
|
Si |
≤1.00 |
≤1.00 |
|
Mn |
≤1.00 |
≤1.00 |
|
P |
≤0.020 |
— |
|
S |
≤0.015 |
≤0.015 |
|
Ni |
≥65.00 |
Balance |
|
Cr |
18.00~21.00 |
18.00~21.00 |
|
Ti |
1.80~2.70 |
1.80~2.70 |
|
Al |
1.00~1.80 |
1.00~1.80 |
|
Co |
≤1.00 |
≤2.00 |
|
Fe |
≤1.50 |
≤3.00 |
|
Cu |
≤0.20 |
≤0.20 |
|
B |
≤0.008 |
≤0.008 |
|
Zr |
— |
≤0.15 |
|
Pb |
— |
≤0.0025 |
Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1
Quick Details
GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,
Delivery
- Delivery status: Forged 、Solutioned 、
- Surface: Polished 、
- Standard: ASTM
- Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other
Inventory Status
| Product type | Products | Dimension | Processes |
|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded |
Product Details
GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,