ISO X2CrNiMo17-12 Enquiry | Print this page
ISO X2CrNiMo17-12 Details
Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes
ISO X2CrNiMo17-12 Standard Download
X2CrNiMo17-12 Datasheet
ISO X2CrNiMo17-12Category | Type | Grade | Microstructure | Designations |
---|---|---|---|---|
Grades | Stainless Steels | X2CrNiMo17-12 | Austenite | International - ISO , ISO 9327-5 (1999) - Steel forgings and rolled or forged bars for pressure purposes - Technical delivery conditions - Part 5: Stainless steels ISO 9329-4 (1997) - Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 4: Austenitic stainless steels ISO 9330-6 (1997) - Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes |
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.030 | ||
Cr | 16.50 | 18.50 | ||
Mo | 11.00 | 14.00 | ||
Ni | 2.00 | 2.50 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
712 (≥) | 468 (≥) | 14 | 43 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
448 (≥) | 243 (≥) | 42 | 41 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
975 | 962 | 398 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
X2CrNiMo17-12-2 | DIN | Germany | DIN 1654-5 (1989) Cold heading and cold extruding steels; technical delivery conditions for stainless steels; Replaced by DIN EN 10263-5:2002 |
1.4404 | DIN | Germany | DIN 1654-5 (1989) Cold heading and cold extruding steels; technical delivery conditions for stainless steels; Replaced by DIN EN 10263-5:2002 |
X2CrNiMo17-13-2 | DIN | Germany | DIN 1654-5 (1989) Cold heading and cold extruding steels; technical delivery conditions for stainless steels; Replaced by DIN EN 10263-5:2002 |
X2CrNiMo17-12-2 | B.S. | UK | Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties |
1.4404 | B.S. | UK | Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties |
X2CrNiMo17-12-3 | B.S. | UK | Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel |
1.4432 | B.S. | UK | Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel |
X2CrNiMo17-12-2 | AFNOR | France | Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel |
1.4404 | AFNOR | France | Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel |
X2CrNiMo17-12-2 | ISO | International | Stainless steels - Chemical composition |
X2CrNiMo17-12-3 | ISO | International | Stainless steels - Chemical composition |
X2CrNiMo17-12 | ISO | International | Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes |
X2CrNiMo17-12 | ISO | International | Welded steel tubes for pressure purposes - Technical delivery conditions - Part 6: Longitudinally welded austenitic stainless steel tubes |
X3CrNiMo17-13-3, 1.4436, X2CrNiMo18-14-3, 1.4435, 1.4432, X2CrNiMo17-12-3 | Whole | Whole | The products in these steel grades are commonly used in the manufacture of pumps, tanks for chemicals, pipelines and installations, heat exchangers, screws, nuts, special coolers, food, chemical, textile, paper and cryogenic equipment, oil and marine indu |