AFNOR X2CrNiN18-7 Enquiry | Print this page
AFNOR X2CrNiN18-7 Details
                          Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel                          
 
                            
                            AFNOR X2CrNiN18-7 Standard Download
X2CrNiN18-7 Datasheet
AFNOR X2CrNiN18-7| Category | Type | Grade | Microstructure | Designations | 
|---|---|---|---|---|
| Grades | Stainless Steels | X2CrNiN18-7 | Austenite | France - AFNOR ,    NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels  NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes NF EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes NF EN 10296-2 (2005) - Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel  | 
                  
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks | 
|---|---|---|---|---|
| C | - | 0.030 | ||
| Si | - | 1.00 | ||
| Mn | - | 2.00 | ||
| P | - | 0.045 | ||
| S | - | 0.015 | ||
| Cr | 16.50 | 18.50 | ||
| Mo | - | - | ||
| Ni | 6.00 | 8.00 | ||
| N | 0.10 | 0.20 | 
| Proof strength Rp0.2 (MPa)  | 
                      Tensile strength Rm (MPa)  | 
                      Impact energy KV (J)  | 
                      Elongation at fracture A (%)  | 
                      Reduction in cross section on fracture Z (%)  | 
                      As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 526 (≥) | 841 (≥) | 42 | 44 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 | 
| Property | Density kg/dm3  | 
                      Temperature T °C/F  | 
                      Specific heat J / kgK  | 
                      Thermal conductivity W/mK  | 
                      Electric resistance µΩ·cm  | 
                      Modulus of elasticity kN/mm2  | 
                      Expansion rate | 
|---|---|---|---|---|---|---|---|
| 465 (≥) | 569 (≥) | 23 | 33 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
| Temp. °C/°F  | 
                      Creep strain limit (10000h) (Rp1,0) N/mm2  | 
                      Creep rupture strength (10000h) (Rp1,0) N/mm2  | 
                      |||||
| 195 | 557 | 526 | 
| Product type | Products | Dimension | Processes | Deliver Status | 
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting | 
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, | 
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting | 
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED | 
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X2CrNiN18-7 | AWS | Germany | Cold heading and cold extruding steels; technical delivery conditions for stainless steels  | 
                  
| X2CrNiN18-7 | AFNOR | France | Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel  | 
                  
| 1.4318 | AFNOR | France | Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel  | 
                  
| X2CrNiN18-7 | ISO | International | Stainless steels - Chemical composition  | 
                  