GBT NS112 Enquiry | Print this page
Category | Type | Steel grade | Standard | Country |
---|---|---|---|---|
Grades | Special Alloy | NS112 | GBT | China |
Chemical composition % of the ladle analysis of grade NS112
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) | Al(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|
0.05-0.10 | Max 1.00 | Max 1.50 | Max 0.030 | Max 0.015 | 19.0-23.0 | 30.0-35.0 | Max 0.75 | 0.15-0.60 | 0.15-0.60 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
137 (≥) | 347 (≥) | 13 | 32 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
945 (≥) | 235 (≥) | 14 | 42 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
782 | 478 | 358 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |