EN EN X5CrNiCuNb16-4 Enquiry | Print this page
Category | Type | Steel grade | Standard | Country |
---|---|---|---|---|
Grades | Special Alloy | EN X5CrNiCuNb16-4 | EN | Euronorm |
Chemical composition % of the ladle analysis of grade EN X5CrNiCuNb16-4
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Nb(%) |
---|---|---|---|---|---|---|---|---|---|
0.070 | 0.70 | 1.50 | 0.040 | 0.015 | 15.0-17.0 | 3.00-5.00 | Max 0.60 | 3.00-5.00 | 5XC-0.45 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
937 (≥) | 785 (≥) | 12 | 44 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
734 (≥) | 258 (≥) | 22 | 31 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
445 | 951 | 424 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
X5CrNiCuNb16-4 | EN | Euronorm | Open die steel forgings for general engineering purposes - Part 4: Stainless steels |
1.4542 | EN | Euronorm | Open die steel forgings for general engineering purposes - Part 4: Stainless steels |
X5CrNiCuNb16-4 | EN | Euronorm | Open die steel forgings for general engineering purposes - Part 4: Stainless steels |
1.4542 | EN | Euronorm | Open die steel forgings for general engineering purposes - Part 4: Stainless steels |
X5CrNiCuNb16-4 | EN | Euronorm | Stainless steels - Chemical composition |
17-4PH, 1.4542, X5CrNiCuNb16-4 | EN | Euronorm | Steel, Corrosion-Resistant, Investment Castings 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu Homogenization, Solution, and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength (17-4) |