GBT 12Cr3MoVSiTiB Enquiry | Print this page
Category | Type | Steel grade | Standard | Country |
---|---|---|---|---|
Grades | Special Alloy | 12Cr3MoVSiTiB | GBT | China |
Chemical composition % of the ladle analysis of grade 12Cr3MoVSiTiB
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Ti(%) |
---|---|---|---|---|---|---|---|
0.09-0.15 | 0.60-0.90 | 0.50-0.80 | 0.03 | 0.03 | 2.50-3.00 | 1.00-1.20 | 0.22-0.38 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
953 (≥) | 972 (≥) | 13 | 14 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
441 (≥) | 787 (≥) | 32 | 14 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
976 | 875 | 239 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |