KS STS410TKA Enquiry | Print this page
Category | Type | Steel grade | Standard | Country |
---|---|---|---|---|
Grades | Special Alloy | STS410TKA | KS | Korea |
Chemical composition % of the ladle analysis of grade STS410TKA
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Nb(%) |
---|---|---|---|---|---|---|---|
Max 0.15 | Max 1.00 | Max 1.00 | Max 0.04 | Max 0.03 | 11.5-13.5 | Max 0.60 | Min 10xC% |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
238 (≥) | 998 (≥) | 41 | 13 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
442 (≥) | 121 (≥) | 12 | 34 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
448 | 977 | 747 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
STS410TKA | KS | Korea | Stainless steel pipes for machine and structural purposes |