Z13C13 Application:Stainless Steel Plate & Steel Strip
Category Type Steel grade Standard Country
Grades Special Alloy Z13C13 AFNOR France

Chemical composition % of the ladle analysis of grade Z13C13

C(%) Si(%) Mn(%) P(%) S(%) Cr(%)
0.10-0.15 Max 0.75 Max 1.00 Max 0.040 Max 0.015 12.0-13.5
Z13C13
Mechanical properties of grade Z13C13
Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
455 (≥) 219 (≥) 13 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Physical properties of grade Z13C13
Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
651 (≥) 816 (≥) 33 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
589 833 449
Z13C13 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED
Cross Reference Table(Equivalent Grade)
Grade Standard Country Application
Z13C13 AFNOR France
Iron and steel. Stainless steel for high temperature application
Z13C13CI AFNOR France
Iron and steel. Cutlery stainless steel