Chemical composition % of the ladle analysis of grade 11Р3АМ3Ф2
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) | W(%) | N(%) | Cu(%) | Co(%) | Nb(%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
1.02-1.12 | 0.20-0.50 | 0.20-0.50 | ≤0.030 | ≤0.030 | 3.80-4.40 | ≤0.60 | 2.50-3.00 | 2.30-2.70 | 2.50-3.30 | 0.05-0.10 | ≤0.25 | ≤0.50 | 0.05-0.20 |
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
874 (≥) | 142 (≥) | 31 | 44 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
875 (≥) | 255 (≥) | 42 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
116 | 298 | 133 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |